Description / Abstract:
The scope of this document is to define a test method for
performing the Compression Stress Relaxation (CSR) Test with the
Automotive Standard (ASD) CSR Jig using the appropriate test
fixtures, configurations and procedures. This standard defines the
equipment needed, guidelines for running the test, and the format
for generating the results and analyzing the data.
Purpose
This document describes test procedures and conditions for
determining the loss in counter-force of a 12.7 mm (0.500 in)
diameter button compressed in an ASD CSR Jig at a constant
deformation, measured at room temperature at periodic intervals,
after exposure to elevated temperatures and/or fluids. It is
designed for testing of vulcanized rubber and thermoplastic
elastomers with an instantaneous Type A Hardness from 45 to 90
(ASTM D2240). Samples are molded and cured in accordance with ASTM
D3182. This document is specific to the use of the ASD CSR jig, a
required apparatus list, a specific test method including a quality
check for the total system. This document was developed based on
testing new and aged specimens. This method can involve hazardous
materials, operations and equipment. This method does not propose
to address all the safety problems associated with its use. It is
the responsibility of user of this method to establish appropriate
safety and health practices and determine the applicability of
regulatory limitations prior to use